Cracked vessels

 

As my porcelain Nerikomi work gets bigger and taller, I have more pots that cracked after final firing, at 1200 degrees, result of stress build up in the layering of coloured porcelain technique. At the moment, over half develop cracks!

This year, this Nerikomi pattern has the most cracking problem, out of 5 pieces fired, only this one survived!


Embrace, Nerikomi 'Lightning'